Today, we loaded 2x40HQ export to Vietnam.
One is SHJ-50 twin screw extruder, the other is SHJ-72 twin screw extruders. Both extruders are used for making filler masterbatch.
Nanjing Jieya is a leading manufacturer of twin screw compounding extruders with over 20 years experience. We will offer you the top quality with best price.
We warmly welcome your inquiry.
The extrusion technology used by the single screw extruder is making waves in the food production industry. We know that single screw extruder can mass produce enterprise products of various shapes and textures. It allows a seamless and continuous operation process, which means that this means lower costs and higher production and sales.
What are the reasons and solutions for the poor discharge or blockage of the single screw extruder head?
What is the importance of single screw extruder temperature control?
What is the importance of single screw extruder speed control?
1. Reasons: (1) A certain section of the heater does not work, and the material is poorly plasticized. (2) The operating temperature is set too low, or the molecular weight distribution of the plastic is wide and unstable. (3) There may be foreign objects in the single screw extruder that are not easy to melt.
2. Treatment method: (1) Check the heater and replace it if necessary. (2) Verify the set temperature of each section, negotiate with the technician if necessary, and increase the temperature set value. (3) Clean and check the extrusion system and head of the single screw extruder.
Temperature control refers to the temperature of the single screw extruder during plastic extrusion, including the temperature control of the barrel, die and transition body. These temperature controls are related to the viscosity of the material, the sensitivity to temperature, and the aggregation state of the polymer. In general, the temperature of the die head and transition body of single screw extruder is low for medium and low viscosity materials, and the temperature of die head and transition body for high viscosity materials is high, and the fluidity is good.
Speed control means that for single screw extrude processing, if the screw speed increases, the shear rate increases. Thermoplastic melts are mostly non-Newtonian pseudoplastic fluids, and their viscosity decreases with the increase of shear rate, and fluidity Increasing the extrusion output also increases. However, if the shear rate is too large, the melt viscosity is too low, which will cause difficulties in the production and operation of single screw extrude. At the same time, the low-viscosity melt will flow backwards under the action of the screw back pressure, and the leakage flow will increase significantly, which will affect the output to a certain extent. , Again, the screw may even slip at high speeds, so the screw speed should be controlled within a certain range. In addition, in the production process of single screw extrude, the screw speed should be kept as stable as possible to avoid fast and slow. Otherwise, it will cause uneven discharge due to excessive changes in the melt viscosity of the material, which will affect normal production.
Nanjing JlEYA is a single screw extruder manufacturer established for more than five years. We work with customers from design to completion to ensure that all technical requirements are met.
The plastic extruder is a common plastic machinery equipment, in the process of the daily operation of the extruder, the extruder will have a variety of failures, affecting the normal production of plastic machinery, the following we will analyze the extruder failure.
Here is the content list:
Unstable host current
The main motor can not start
The head is not discharged smoothly or blocked
The main electric starting current is too high
The main motor makes an abnormal sound
1. Production reasons.
(1) Uneven feeding.
(2) The main motor bearing of the plastic extruder is damaged or poorly lubricated.
(3) A section of the heater is out of order and does not heat up.
(4) The screw adjustment pad is not correct, or the phase is not correct, and the component interferes.
2. Treatment methods.
(1) Check the feeder, troubleshooting.
(2) Overhaul the main motor of the plastic extruder, replace the bearings if necessary.
(3) Check whether each heater is working properly, replace the heater if necessary.
(4) Check the adjustment pad, pull out the screw to check whether there is interference with the screw.
1. Causes.
(1) There is a mistake in the start-up procedure of the plastic extruder.
(2) The main motor thread has a problem, whether the fuse is burned ring.
(3) The main motor-related chain device to function
2. Treatment methods.
(1) Check the program, reboot the machine in the correct boot sequence.
(2) Check the main motor circuit.
(3) Check whether the lube oil pump of the plastic extruder is started and check the status of the chain device associated with the main motor. The oil pump is not on and the motor cannot be turned on.
(4) The inverter induction power has not been discharged. Turn off the main power and wait for 5 minutes before starting again.
(5) Check whether the emergency button is reset.
1. Causes.
(1) A section of the heater does not work, and the material is not plasticized well.
(2) The operating temperature setting is low, or the molecular weight distribution of plastic is wide and unstable.
(3) There may be foreign substances that do not melt easily.
2. Treatment methods.
(1) Check the heater of the plastic extruder and replace it if necessary.
(2) Verify the set temperature of each section, and if necessary, consult with the technician to increase the temperature setting.
(3) Clean and check the extrusion system and the head.
1. Causes.
(1) Insufficient heating time and high torque.
(2) A section of the heater does not work.
2. Treatment methods.
(1) Apply hand pan machine when starting, if not easy, extend the heating time or check whether each section heater is working properly.
1. Produced by.
(1) The main motor bearing of the plastic extruder is damaged.
(2) The main motor silicon controlled rectifier line in silicon controlled damage.
2. Treatment methods.
(1) Replace the main motor bearings.
(2) Check the silicon-controlled rectifier circuit, if necessary, replace the silicon-controlled components.
Our company's website is https://www.njjyextrusion.com/. If you still have questions, you can contact us on the official website.
Twin screw extruder is developed based on the single screw extruder, which has been widely used in the molding process of extruded products because of its good feeding performance, mixing and plasticizing performance, exhaust performance, and extrusion stability. So what are the advantages of a twin screw extruder? The following is a detailed introduction.
Here is the content list:
l Wear and tear
l Reduce production costs
l Increase output
l Improve labor efficiency
l High torque and high speed
Wear and tear
Since twin screw extruders are easy to open, the degree of wear of threaded elements and barrel bushings can be detected at any time, so that effective repair or replacement can be carried out. It is not necessary to find out only when there is a problem with the extruded product, which causes unnecessary waste.
Reduce production costs
When producing masterbatches on twin screw extruders, it's usually necessary to alter colors, and if a product amendment is critical, to open the open process space within several minutes, in addition to analyzing the mixing process by looking at the melt profile on the entire screw. The current common twin screw extruder needs to be cleared with a large amount of clearing material when changing colors, which is time consuming, power consuming, and a waste of raw material. The split twin screw extruder can solve this problem. When changing the color, it only takes a few minutes to quickly open the barrel for manual cleaning, so that no or less cleaning material can be used, saving costs.
Increase output
Twin screw snack extruders use side feeding technology to improve the integrity of the material and greatly increase production. The position and shape of the feed opening also have a great influence on feeding efficiency. With the same parameters, the output increases with an increase in the feed area. A rectangular cross section has a higher feed efficiency than a circular cross section for the same inlet area. The use of side by side twin screw feeds is also based on this consideration.
Improve labor efficiency
During equipment maintenance, ordinary twin screw extruders often have to remove the heating and cooling system before the screw can be withdrawn as a whole. In contrast, the split twin screw does not need to be opened by loosening a few bolts and turning the worm gearbox handle device to lift the upper half of the barrel, and then the entire barrel can be repaired. This shortens the maintenance time and reduces the labor intensity.
High torque and high speed
At present, the event trend of twin screw extruders within the world is to develop within the direction of high torsion, high speed, and low energy consumption, and also the impact of high speed is high productivity. The split twin screw extruder belongs to the current class, and its speed will reach and five hundred revolutions per minute. Therefore, its distinctive benefits in process high viscousness and warmth sensitive materials.
In the high speed, high torque core technology, asymmetric and symmetric high torque gearbox currently only Germany and Japan related manufacturers master the core technology, its speed can reach up to 1800 rpm or more, and domestic also master this core technology, such as Nanjing JlEYA extrusion company, is also currently one of the main choices of domestic high end material processing manufacturers, belongs to the domestic independent innovation national encouragement projects.
If you want to buy twin screw extruders, you can consider our cost effective products. We insist on the tenet of "quality first, customer first" and warmly welcome new and old customers to cooperate with us.
The company focuses on twin screw extruders, micro twin screw extruders, plastic extruders, parallel twin screw extruders, and other research and development and manufacturing as the core of the isotropic rotary twin screw mixing and extruding machine, the application range covers the mixing and modification of granulation, polymerization, deswelling, step molding, recycling, and other fields.
The screw can be said to be the heart of the injection molding machine. The quality of the screw determines the quality of the product. The plasticizing screw of the engineering plastic twin screw extruder has the functions of conveying, melting, mixing, compression, metering and exhausting. It plays an important role in the quality of plasticization and is a key factor affecting the quality of plasticization.
What is the difference between engineering plastic twin screw extruder and single screw extruder?
What are the characteristics of engineering plastic twin screw extruder?
What are the structural principles of engineering plastic twin screw extruder?
1. Price: single screw extruder has simple structure and low price; Engineering plastic twin screen expander is complex and expensive
2. Plasticizing capacity: single screw extruder is suitable for plasticizing and extruding polymers and granular materials. The shear degradation of polymer is small, but the residence time of material in extruder is long; The engineering plastic twin screw extruder has good mixing and plasticizing ability, and the residence time of materials in the extruder is short, which is suitable for powder processing.
3. In terms of processing capacity and energy consumption: the engineering plastic twin screw extruder has large output, fast extrusion speed and low energy consumption per unit output, while the single screw extruder is poor.
4. Operability: the single screw extruder is easy to operate and the process control is simple; The operation of engineering plastic twin screen expander is relatively complex and the process control requirements are high.
1. engineering plastic twin screw extruder is divided into parallel and conical according to the relative position of the two axes;
2. engineering plastic twin screw extruder is divided into meshing type and non-meshing type according to the two screw meshing procedures;
3. engineering plastic twin screw extruder is divided into the same direction and the opposite direction according to the rotation direction of the two screws, and there are inward and outward points in the opposite direction;
4. engineering plastic twin screw extruder is divided into high speed and low speed according to the screw rotation speed;
5. engineering plastic twin screw extruder is divided into whole and combination according to the structure of screw and barrel.
For the basic mechanism of the engineering plastic twin screw extruder process, in simple terms, a screw rotates in the barrel and pushes the plastic forward. The screw structure is an inclined surface or slope wound on the center layer, the purpose of which is to increase the pressure in order to overcome the greater resistance. As far as the engineering plastic twin screw extruder is concerned, there are three kinds of resistance that need to be overcome during work: one is friction, which includes the friction of solid particles (feeding) against the barrel wall and the first few revolutions of the screw (feeding zone). There are two kinds of mutual friction forces; the second is the adhesion of the melt on the cylinder wall; the third is the internal logistics resistance of the melt when it is pushed forward.
Nanjing JlEYA has focused on the development and production of engineering plastic twin screw extruders for several years. And it commits to provide perfect service for every customer from all over the world.
The engineering plastic twin screw extruder consists of a transmission device, a feed device, a barrel, and a screw. The function of each component is similar to that of a single-screw extruder. The difference to the single screw extruder is that in the engineering plastic twin screw extruder two parallel snails are arranged in the "cross-section" of the material.
What is the working principle of the engineering plastic twin screw extruder?
How do you treat a engineering plastic twin screw extruder?
Why is the cooling device particularly important when using engineering plastic twin screw extruders?
From the point of view of the principle of movement, the engineering plastic twin screw extruder distinguishes between the straight and uneven, and non-foaming types.
1. Double screw extruder of technical plastic
This type of engineering plastic twin screw extruder has a low speed and a high speed. The former is mainly used for profile extraction, while the latter is used for special polymer processing operations.
(1) Tightly machined extruder. The slow-running extruder has a closely combining screw geometry, in which the spiral antenna shape of one snail closely matches the spiral antenna shape of the other snail, i.e. the conjugated snail shape.
(2) Self-cleaning extruder. The simultaneous high-speed extruder has a closely tuned spiral shape. This type of snail can be executed with a relatively small snail split so that the snail has a closed self-cleaning effect. This type of engineering plastic twin screw extruder is called a compact self-cleaning engineering plastic twin screw extruder.
The gap between the two screw edges of the closely combining, opposing engineering plastic twin screw extruder is very small (much smaller than the gap in the evenly rotating engineering plastic twin screw extruder) so those positive conveying properties can be achieved.
2. Non-reciprocating double screw extruder of technical plastic
The axis distance between the two snails of the non-foaming engineering plastic twin screw extruder is greater than the sum of the radii of the two snails.
1. After using the engineering plastic twin screw extruder for 500 hours, iron chips or other impurities from the gears are in the gearbox. Therefore, the gears should be cleaned and the gear lubricant replaced.
2. The engineering plastic twin screw extruder should carry out a comprehensive inspection of the extruder after an operating period to check the density of all snails.
3. If the double screw extruder is suddenly switched off during production, the main drive, and the heating stops, if the power supply is restored, each section of the cylinder shall be reheated to the specified temperature and kept for a specified period, before you can start the extruder.
4. If the display and the display of the engineering plastic twin screw extruder are full, check if the contact of the thermocouple, etc. is good.
After the molded plastic extrusion layer has left the engineering plastic twin screw extruder, it should be cooled and formed immediately, otherwise, it will deform under the influence of gravity. The cooling method normally uses water cooling and is divided into quick cooling and slow cooling according to the different water temperatures. Fast cooling is the direct cooling by cold water. Rapid cooling is advantageous for the design of the extruded plastic layer, but in the case of crystalline polymers, due to sudden heat cooling, it is easy to leave internal stresses in the extruded layer structure, which leads to cracks during use. Generally PVC The plastic layer is deterred. Slow cooling should reduce the inner tension of the product. Water with different temperatures is given in the cooling water tank to gradually reduce the temperature and shape of the product. The extrusion of PE and PP takes place under slow cooling, i.e. through hot water, hot water, and cold water, which is called three-stage cooling.
Nanjing JlEYA is the leading manufacturer extruder manufacturer specializing in twin screw extrude. If you want to get more information, just go and connect them.
Nanjing JIEYA attend Chinaplas 2021 held in Shenzhen. We sincerely welcome your visiting.
Our booth no.: 7Q25
Time: April 13-16, 2021
Address: Shenzhen World Exhibition Center
Look forward to meet you at there.
![]() | ![]() |
underwater pelletizing machine plays an irreplaceable role in the current industrial production process. Only when the underwater pelletizing machine is used correctly can the greatest effect be achieved.
What problems should be paid attention to when using underwater pelletizing machine?
What is the cause of the friction clutch failure of the underwater pelletizing machine and its solution?
How can the underwater pelletizing machine make the pellets cut out by pelletizing have no pores?
1. Pay attention to the temperature change of the underwater pelletizing machine at any time. When touching the sliver with clean hands, the temperature should be raised immediately. Until the sliver touches your hand, it is normal.
2. When the bearing part of the reducer burns, or is accompanied by noise, it should be repaired in time and refueled.
3. When the bearing parts at both ends of the bearing chamber of the underwater pelletizing machine are hot or there is noise, stop the machine for maintenance and add butter. During normal operation, add butter to the bearing chamber every 5-6 days.
4. Pay attention to the operating rules of the underwater pelletizing machine; such as: the machine temperature is high or low, the speed is fast or slow, and it can be dealt with in time according to the situation.
5. When the operation of the underwater pelletizing machine is unstable, pay attention to check whether the gap of the coupling anastomosis is too tight, and adjust it in time to loosen it.
Reason analysis: The instantaneous starting voltage of the main motor of the underwater pelletizing machine is too low, the friction disc and the friction disc are overheated, the friction disc and the friction disc are aging, and the air pressure of the friction disc is too low, etc., which can cause the clutch to disengage.
Solution: When starting the main motor of the underwater pelletizing machine, avoid peak power consumption and reduce the feeding load. The minimum restart interval is 30 minutes; in summer, when the main motor is restarted more than twice, it should be extended. Interval time or forced cooling with a fan. Blow with instrument wind and wipe off the dirt on the surface of the friction plate and friction plate with a rag. If the underwater pelletizing machine wears a lot or the surface becomes "vitrified", replace the friction plate and friction plate. Confirm whether the air pressure value can make the friction disc and the friction plate fit together.
One: The different materials used by the underwater pelletizing machine must be separated clearly;
Two: The products produced by the underwater pelletizing machine should be dewatered as much as possible after being crushed and cleaned;
Three: The vent hole on the screw of the underwater pelletizing machine should be unblocked.
Nanjing JlEYA has various underwater pelletizing machines that can provide the increasing of products, and make them more effective, reliable, and consistent.